Characterization of anodic aluminum oxide film and its application to amorphous silicon thin film transistors
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.citation.epage |
172 | en_US |
dc.citation.issue |
2 | en_US |
dc.citation.spage |
166 | en_US |
dc.citation.volume |
43 | en_US |
dc.citation.woscount |
9 | |
dc.contributor.author |
Liang, CW | en_US |
dc.contributor.author |
Luo, TC | en_US |
dc.contributor.author |
Feng, MS | en_US |
dc.contributor.author |
Cheng, HC | en_US |
dc.contributor.author |
Su, D | en_US |
dc.contributor.department |
材料科學與工程學系 | zh_TW |
dc.contributor.department |
電子工程學系及電子研究所 | zh_TW |
dc.contributor.department |
奈米中心 | zh_TW |
dc.contributor.department |
Department of Materials Science and Engineering | en_US |
dc.contributor.department |
Department of Electronics Engineering and Institute of Electronics | en_US |
dc.contributor.department |
Nano Facility Center | en_US |
dc.date.accessioned |
2014-12-08T15:02:51Z | |
dc.date.available |
2014-12-08T15:02:51Z | |
dc.date.issued |
1996-02-01 | en_US |
dc.description.abstract |
AL(2)O(3)/SINx double-layered dielectric films suitable for large-size amorphous silicon thin film transistor liquid crystal displays (a-Si:H TFT LCD) have been prepared by anodization and plasma enhanced chemical vapor deposition (PECVD). Al2O3 films were formed at various pH values and volume ratio of water (H2O%) in the electrolyte. The optimal quality of Al2O3 film was achieved at pH = 6 and H2O% = 30. These high-quality Al2O3 films have denser structure, lower etching rate (90 Angstrom min(-1)) and smooth surface morphology after etching. The capacitors made of the anodization show a breakdown field as high as 7.8 MV cm(-1) and a low leakage current density of 10 nA cm(-2) at a dielectric field of 3 MV cm(-1). Furthermore, a-Si:H TFTs with Al gate and different gate dielectrics (Al2O3/SINx and SiNx) were also fabricated and evaluated. The TFTs with Al2O3/SiNx double-layered gate dielectric provide better performances, such as the smaller threshold voltage (1.76 V), improved subthreshold swing (1.0 V dec(-1)), and lower off-current (3.8 PA) than those of the device with single SiNx, film. | en_US |
dc.identifier.doi |
10.1016/0254-0584(95)01619-6 | en_US |
dc.identifier.issn |
0254-0584 | en_US |
dc.identifier.journal |
MATERIALS CHEMISTRY AND PHYSICS | en_US |
dc.identifier.uri |
http://dx.doi.org/10.1016/0254-0584(95)01619-6 | en_US |
dc.identifier.uri |
https://ir.lib.nycu.edu.tw/handle/11536/1461 | |
dc.identifier.wosnumber |
WOS:A1996TZ39800013 | |
dc.language.iso |
en_US | en_US |
dc.subject |
anodization | en_US |
dc.subject |
Al2O3 | en_US |
dc.subject |
amorphous silicon | en_US |
dc.subject |
thin film transistor | en_US |
dc.title |
Characterization of anodic aluminum oxide film and its application to amorphous silicon thin film transistors | en_US |
dc.type |
Article | en_US |
檔案
- A1996TZ39800013.pdf (1.01 MB, Adobe PDF)
所屬典藏: 期刊論文
引用此條目
Liang, C., Luo, T., Feng, M., Cheng, H., & Su, D. (1996). Characterization of anodic aluminum oxide film and its application to amorphous silicon thin film transistors. MATERIALS CHEMISTRY AND PHYSICS, 43(2), 166–172. https://doi.org/10.1016/0254-0584(95)01619-6
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/1461