Breakdown characteristics of ultra-thin gate oxides caused by plasma charging
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.citation.epage |
319 | en_US |
dc.citation.spage |
313 | en_US |
dc.citation.volume |
567 | en_US |
dc.contributor.author |
Chen, CC | en_US |
dc.contributor.author |
Lin, HC | en_US |
dc.contributor.author |
Chang, CY | en_US |
dc.contributor.author |
Chien, CH | en_US |
dc.contributor.author |
Huang, TY | en_US |
dc.contributor.department |
電子工程學系及電子研究所 | zh_TW |
dc.contributor.department |
Department of Electronics Engineering and Institute of Electronics | en_US |
dc.date.accessioned |
2014-12-08T15:27:09Z | |
dc.date.available |
2014-12-08T15:27:09Z | |
dc.date.issued |
1999 | en_US |
dc.description.abstract |
Breakdown characteristics of ultra-thin gate oxides caused by plasma charging were studied in this work. It is observed that as oxide thickness is scaled down to 4 nn, some traditional monitor parameters may lose their sensitivity for detecting oxide degradation induced by plasma charging damage, due to insignificant trap generation. Even the gate leakage current, although sensitive for 4 nm oxide, may no longer be sensitive enough for even thinner oxide (e.g., 2.6 nm), due to the existence of large tunneling current. Moreover, several soft-breakdown events were found to occur in ultrathin oxide before the final onset of a catastrophic hard-breakdown. Finally, an equivalent local oxide thickness is calculated using local oxide thinning model to estimate the stepwise increase of gate current after soft-breakdown event. | en_US |
dc.identifier.isbn |
1-55899-474-2 | en_US |
dc.identifier.issn |
0272-9172 | en_US |
dc.identifier.journal |
ULTRATHIN SIO2 AND HIGH-K MATERIALS FOR ULSI GATE DIELECTRICS | en_US |
dc.identifier.uri |
https://ir.lib.nycu.edu.tw/handle/11536/19393 | |
dc.identifier.wosnumber |
WOS:000082728600044 | |
dc.language.iso |
en_US | en_US |
dc.title |
Breakdown characteristics of ultra-thin gate oxides caused by plasma charging | en_US |
dc.type |
Proceedings Paper | en_US |
檔案
本條目沒有附加檔案。
所屬典藏: 會議論文
引用此條目
Chen, C., Lin, H., Chang, C., Chien, C., & Huang, T. (1999). Breakdown characteristics of ultra-thin gate oxides caused by plasma charging. ULTRATHIN SIO2 AND HIGH-K MATERIALS FOR ULSI GATE DIELECTRICS, 567, 313–319. https://ir.lib.nycu.edu.tw/handle/11536/19393
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。