Investigation on plasma treatment for transparent Al-Zn-Sn-O thin film transistor application
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.citation.epage |
41 | en_US |
dc.citation.issue |
en_US | |
dc.citation.spage |
36 | en_US |
dc.citation.volume |
549 | en_US |
dc.citation.woscount |
0 | |
dc.contributor.author |
Chang, Chih-Hsiang | en_US |
dc.contributor.author |
Liu, Po-Tsun | en_US |
dc.contributor.department |
光電工程學系 | zh_TW |
dc.contributor.department |
顯示科技研究所 | zh_TW |
dc.contributor.department |
Department of Photonics | en_US |
dc.contributor.department |
Institute of Display | en_US |
dc.date.accessioned |
2014-12-08T15:33:23Z | |
dc.date.available |
2014-12-08T15:33:23Z | |
dc.date.issued |
2013-12-31 | en_US |
dc.description.abstract |
This work reported the physical characteristics and electrical performance of amorphous Al-Zn-Sn-O thin film transistor (a-AZTO TFT) device under the temperature effects of thermal annealing process and various gas plasma post-treatments. The thermal annealing at 450 degrees C could strengthen the oxygen bonding of a-AZTO film, thereby improving the film quality and TFT device performance. In addition, the oxygen deficient can be reduced effectively by the O-2 and N2O plasma treatments, respectively, leading to enhanced electrical reliability. Also, the optical energy gap of a-AZTO films with O-2 or N2O plasma treatment was measured about 3.5 eV, which indicated that all of the a-AZTO films were insensitive to visible light. On the other hand, the electron mobility of a-AZTO TFT was observed to be promoted after NH3 plasma post-treatment. The improvement could be attributed to a slight doping effect of H+ ions. These results showed the potential of post-treatments for flat panel displays applications of transparent a-AZTO TFT technology. (C) 2013 Elsevier B. V. All rights reserved. | en_US |
dc.identifier.doi |
10.1016/j.tsf.2013.06.042 | en_US |
dc.identifier.issn |
0040-6090 | en_US |
dc.identifier.journal |
THIN SOLID FILMS | en_US |
dc.identifier.uri |
http://dx.doi.org/10.1016/j.tsf.2013.06.042 | en_US |
dc.identifier.uri |
https://ir.lib.nycu.edu.tw/handle/11536/23199 | |
dc.identifier.wosnumber |
WOS:000327537100008 | |
dc.language.iso |
en_US | en_US |
dc.subject |
Thermal annealing | en_US |
dc.subject |
AlZnSnO TFT | en_US |
dc.subject |
Plasma post treatment | en_US |
dc.subject |
Oxygen bonding | en_US |
dc.subject |
Reliability mechanism | en_US |
dc.title |
Investigation on plasma treatment for transparent Al-Zn-Sn-O thin film transistor application | en_US |
dc.type |
Article | en_US |
檔案
- 000327537100008.pdf (1.55 MB, Adobe PDF)
所屬典藏: 期刊論文
引用此條目
Chang, C.-H., & Liu, P.-T. (2013). Investigation on plasma treatment for transparent Al-Zn-Sn-O thin film transistor application. THIN SOLID FILMS, 549, 36–41. https://doi.org/10.1016/j.tsf.2013.06.042
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/23199