The effect of oxygen-to-argon ratio on the electrical and reliability characteristics of sputtered Sr0.8Bi2.5Ta1.2Nb0.9O9+x thin films
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.citation.epage |
199 | en_US |
dc.citation.issue |
1-2 | en_US |
dc.citation.spage |
190 | en_US |
dc.citation.volume |
372 | en_US |
dc.citation.woscount |
7 | |
dc.contributor.author |
Tsai, MS | en_US |
dc.contributor.author |
Tseng, TY | en_US |
dc.contributor.department |
電子工程學系及電子研究所 | zh_TW |
dc.contributor.department |
Department of Electronics Engineering and Institute of Electronics | en_US |
dc.date.accessioned |
2014-12-08T15:44:55Z | |
dc.date.available |
2014-12-08T15:44:55Z | |
dc.date.issued |
2000-08-22 | en_US |
dc.description.abstract |
This work investigated how the annealing process affects the ferroelectric properties of thin films of Sr0.8Bi2.5Ta1.2Nb0.9O9+x (SBTN) on Ir/SiO2/Si substrates prepared by two-target off-axis rf magnetron sputtering at various O-2/(Ar + O-2) mixing ratios (OMR) with a substrate temperature of 570 degrees C. Experimental results indicated that the annealing could effectively result in a large remanent polarization. The remanent polarization, dielectric constant and leakage current of 598 degrees C post-annealing SBTN thin films increased with an increase in the OMR and reached a maximum value at 40% OMR. In addition, the results obtained from the dielectric constant and the leakage current were interpreted in terms of polarization effect and loss theory. The 400-nm thick 40% OMR SBTN films with 598 degrees C post-annealing exhibited good surface morphology and had a dielectric constant of 752, a loss tangent of 0.035 at 100 kHz, a leakage current density of 6 x 10(-6) A/cm(2) at an electric field of 50 kV/cm with a delay time of 30 s, a remanent polarization (2P(r)) of 40 mu C/cm(2), a coercive field (2E(c)) of 77 kV/cm at an applied voltage of 3 V, and a measured value of Q(sw) of 20 mu C/cm(2). According to studies on the 10-year lifetime of time-dependent dielectric breakdown (TDDB), high OMR samples have a longer lifetime than the other lower OMR samples. The SBTN films demonstrated fatigue free characteristics up to 10(11) switching cycles under a 3-V bipolar 1 MHz square wave. Moreover, the polarization of the films decreases slightly (less 0.5% per decade) with retention time up to 240 min. (C) 2000 Elsevier Science S.A. All rights reserved. | en_US |
dc.identifier.doi |
10.1016/S0040-6090(00)01057-9 | en_US |
dc.identifier.issn |
0040-6090 | en_US |
dc.identifier.journal |
THIN SOLID FILMS | en_US |
dc.identifier.uri |
http://dx.doi.org/10.1016/S0040-6090(00)01057-9 | en_US |
dc.identifier.uri |
https://ir.lib.nycu.edu.tw/handle/11536/30326 | |
dc.identifier.wosnumber |
WOS:000089269800026 | |
dc.language.iso |
en_US | en_US |
dc.subject |
sputtering | en_US |
dc.subject |
SBT | en_US |
dc.subject |
reliability | en_US |
dc.subject |
ferroelectric properties | en_US |
dc.title |
The effect of oxygen-to-argon ratio on the electrical and reliability characteristics of sputtered Sr0.8Bi2.5Ta1.2Nb0.9O9+x thin films | en_US |
dc.type |
Article | en_US |
檔案
- 000089269800026.pdf (421.6 KB, Adobe PDF)
所屬典藏: 期刊論文
引用此條目
Tsai, M., & Tseng, T. (2000). The effect of oxygen-to-argon ratio on the electrical and reliability characteristics of sputtered Sr0.8Bi2.5Ta1.2Nb0.9O9+x thin films. THIN SOLID FILMS, 372(1-2), 190–199. https://doi.org/10.1016/S0040-6090(00)01057-9
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/30326