Corrosion behaviors of austenitic Fe-30Mn-7Al-xCr-1C alloys in 3.5% NaCl solution
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.citation.epage |
598 | en_US |
dc.citation.issue |
2-3 | en_US |
dc.citation.spage |
595 | en_US |
dc.citation.volume |
114 | en_US |
dc.citation.woscount |
5 | |
dc.contributor.author |
Tuan, Y. H. | en_US |
dc.contributor.author |
Wang, C. S. | en_US |
dc.contributor.author |
Tsai, C. Y. | en_US |
dc.contributor.author |
Chao, C. G. | en_US |
dc.contributor.author |
Liu, T. F. | en_US |
dc.contributor.department |
材料科學與工程學系 | zh_TW |
dc.contributor.department |
Department of Materials Science and Engineering | en_US |
dc.date.accessioned |
2014-12-08T15:09:37Z | |
dc.date.available |
2014-12-08T15:09:37Z | |
dc.date.issued |
2009-04-15 | en_US |
dc.description.abstract |
The corrosion behaviors of the as-quenched Fe-30wt.%Mn-7wt.%Al-xwt.%Cr-1 wt.%C alloys (x = 0, 3, 6 and 9) in 3.5% NaCl have been investigated. Passivation could be observed for all the alloys except for the alloy without Cr content. The corrosion potential (E(corr)) and pitting potential (E(pp)) increased pronouncedly with increasing Cr content up to 6 wt.%, and decreased as Cr content up to 9 wt.%. The decrease of E(corr) and E(pp) of the alloy containing 9 wt.% Cr was due to the formation of (Fe,Mn,Cr)(7)C(3) carbides in the austenite matrix and on the grain boundaries. It is noted that the corrosion behaviors of the austenitic Fe-Mn-Al-Cr-C alloys with higher Cr(>= 3 wt.%) content have never been reported in previous literatures. (C) 2008 Elsevier B.V. All rights reserved. | en_US |
dc.identifier.doi |
10.1016/j.matchemphys.2008.10.009 | en_US |
dc.identifier.issn |
0254-0584 | en_US |
dc.identifier.journal |
MATERIALS CHEMISTRY AND PHYSICS | en_US |
dc.identifier.uri |
http://dx.doi.org/10.1016/j.matchemphys.2008.10.009 | en_US |
dc.identifier.uri |
https://ir.lib.nycu.edu.tw/handle/11536/7366 | |
dc.identifier.wosnumber |
WOS:000263833500018 | |
dc.language.iso |
en_US | en_US |
dc.subject |
Alloy | en_US |
dc.subject |
Corrosion | en_US |
dc.subject |
Electrochemical techniques | en_US |
dc.subject |
Carbides | en_US |
dc.title |
Corrosion behaviors of austenitic Fe-30Mn-7Al-xCr-1C alloys in 3.5% NaCl solution | en_US |
dc.type |
Article | en_US |
檔案
- 000263833500018.pdf (483.3 KB, Adobe PDF)
所屬典藏: 期刊論文
引用此條目
Tuan, Y. H., Wang, C. S., Tsai, C. Y., Chao, C. G., & Liu, T. F. (2009). Corrosion behaviors of austenitic Fe-30Mn-7Al-xCr-1C alloys in 3.5% NaCl solution. MATERIALS CHEMISTRY AND PHYSICS, 114(2-3), 595–598. https://doi.org/10.1016/j.matchemphys.2008.10.009
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/7366