<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css"> Skip to main content

The combination of rolling-and-T6-treatments with Al2O3-reinforcing-particles effect on A6061 metal-matrix composites

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

DOI

10.1177/1464420714565433

Abstract

Al-Si alloys, with excellent properties such as low weight, low thermal expansion coefficient, and high wear-resistance, are ideal materials for the automobile and aerospace industries. However, their applications have been hampered by the coarsening of the primary-Si particles in Al-Si alloys. In this study, the rolling-and-T6-treatments effect on A6061/Al2O3 metal-matrix composites is investigated. The A6061/Al2O3 metal-matrix composites with different amounts of reinforcing Al2O3 particles are examined in the aspects of wear resistance and hardness. Upon the T6 treatment, the hardness is enhanced in all cases and is summarized. The results suggest that the increase of Al2O3 particles reduce the wear rate. The possible reinforce mechanisms and the environmental temperature effects are discussed. This improvement in wear resistance is due to the particle size refinement of silicon at a high percentage-roll-reduction.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By