Abstract

The vertical organic space-charge-limited transistor made of P3HT and small-molecule phosphorescent organic light-emitting diode (OLED) are made on two separate glass substrate by blade coating, then soldered vertically together by tin balls with 40 mu m diameter. The soldering is done by hot wind of 150 degrees C for 5 min Contact resistance is only 10 Omega. The vertical transistor is annealed at 150 degrees C for 5 min before soldering to enhance the output current up to 25 mA/cm(2) and give high thermal stability. Both OLED and the annealed vertical transistor are not affected by the soldering process. The vertical transistor has 1/4 of the OLED area and turns on the bottom-emission white OLED up to 300 cd/m(2) and orange OLED up to 600 cd/m(2). The entire operation is within 8 V. OLED and transistor array can therefore be made on separate glass substrates then soldered together to form the display. (C) 2013 Elsevier B. V. All rights reserved.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By