Title: ETHANOL REFORMING CATALYST COMPOSITION AND METHOD OF PRODUCING ETHANOL REFORMING CATALYST
Authors: LEE CHI-SHEN
WENG SHENG-FENG
CHEN YUN-SHENG
WANG YUN-HSIN
Issue Date: 31-Jul-2014
Abstract: The instant disclosure relates to a preparation method of ethanol reforming catalyst, comprising the following steps. The first step is mixing a first metal precursor, a second metal precursor, and a third metal precursor with an organic medium to form a mixture. The next step is adding a surfactant to the mixture, and then allowing resting for 3 to 7 days to form a colloidal gel. The next step is calcining the colloidal gel for 1 to 5 hours in a first temperature region of 350° C. to 550° C., and then calcining the colloidal gel for 1 to 5 hours in a second temperature region of 800° C. to 1000° C. to form an ethanol reforming catalyst. The instant disclosure further provides an ethanol reforming catalyst composition.
Gov't Doc #: B01J023/83
URI: http://hdl.handle.net/11536/104882
Patent Country: USA
Patent Number: 20140213440
Appears in Collections:Patents


Files in This Item:

  1. 20140213440.pdf

If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.