MOS devices interface defect density measurements such as the hi-lo CV method and the conductance method are extremely important and widely used. Interface defect response time is a key parameter in both measurements as well as in their interpretations. It is widely accepted that interface defects at energies close to the band edge have too short a response time to be measured properly by these techniques, unless very high measurement frequencies are employed, which greatly increases the experimental difficulty. Consequently, near band edge interface defects are deemed unreliable and generally not reported. Here we show that the time constant of band edge defects has been misunderstood. Specifically, we show that as the capacitor is biased into accumulation – a necessity to measure defect levels near the band edge, the defect response time levels off instead of continuing to decrease. As a result, the commonly available 1MHz measurement frequency is more than adequate even for defects near the band edge.

所屬典藏

期刊論文
顯示完整詮釋資料 統計資料

引用此條目

Cheung, K. P., Wen, Y.-X., & Tsui, B.-Y. (2025). On the Response Time Constant of Interface Defects in Accumulation. IEEE Transactions on Device and Materials Reliability, 26(1), 384–386. https://doi.org/10.1109/tdmr.2025.3635880

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://ir.lib.nycu.edu.tw/handle/11536/192033