摘要
Polycrystalline diamond films were deposited on p-type (100) silicon substrate using a methane/hydrogen gas mixture in a microwave plasma-assisted chemical vapor deposition system. After the back-etched process, the Al contacts were evaporated on both sides of a 150 mum thick isolated diamond film for consecutive high-voltage measurements. It was found that the current-voltage (I-V) characteristics of the Al/diamond/Al structure exhibited two Schottky barrier diodes in a back-to-back configuration. Since the top diamond surface possessed better diamond quality than the bottom surface, the top Schottky diode with a breakdown voltage of 897 V and a lower breakdown voltage of -515 V for the bottom Schottky diode was observed for the first I-V measurement. However, the breakdown voltage was decreased by 37 and 140 V for the top and bottom Schottky diodes after the consecutive sixth repeated measurements. It was found that the oxygenated phenomenon was more prominent; in addition, the quality of the isolated diamond film was also degraded after the consecutive high-voltage measurements. It was indicated that decrease of the breakdown voltage was due to the oxidation layer and the non-diamond components on both surfaces of the isolated diamond film. (C) 2001 Elsevier Science B.V. All rights reserved.
所屬典藏
會議論文引用此條目
Huang, B., Ke, W., Hsu, J., & Chen, W. (2001). Successive current-voltage measurements of a thick isolated diamond film. MATERIALS CHEMISTRY AND PHYSICS, 72(2), 214–217. https://doi.org/10.1016/S0254-0584(01)00439-4
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/29261