Fabrication and characterization of Cu-SiCp composites for electrical discharge machining applications
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.citation.epage |
502 | en_US |
dc.citation.issue |
4 | en_US |
dc.citation.spage |
483 | en_US |
dc.citation.volume |
16 | en_US |
dc.citation.woscount |
17 | |
dc.contributor.author |
Shu, KM | en_US |
dc.contributor.author |
Tu, GC | en_US |
dc.contributor.department |
材料科學與工程學系 | zh_TW |
dc.contributor.department |
Department of Materials Science and Engineering | en_US |
dc.date.accessioned |
2014-12-08T15:44:22Z | |
dc.date.available |
2014-12-08T15:44:22Z | |
dc.date.issued |
2001 | en_US |
dc.description.abstract |
Cu-SiCp composites made by the powder metallurgy method were investigated. To avoid the adverse effect of Cu-SiCp reaction, sintering was controlled at a reaction temperature less than 1032 K. Electroless plating was employed to deposit a copper film on SiCp powder before mixing with Cu powder in order to improve the bonding status between Cu and SiC particles during sintering. It was found that a continuous copper film could be deposited on SiCp by electroless copper plating, and a uniform distribution of SiCp in Cu matrix could be achieved after the sintering and extrusion process. The mechanical properties of Cu-SiCp composites with SiCp contents from 0.6 to 10 wt% were improved evidently, whereas electrical properties remained almost unchanged as compared with that of the pure copper counterpart. In the electrical discharge machining (EDM) test, the as-formed composite electrodes exhibited a character of lower electrode wear ratio, justifying its usage. The optimum conditions for EDM were Cu-2 wt% SiC. composite electrode operating with a pulse time of 150 mu sec. | en_US |
dc.identifier.doi |
10.1081/AMP-100108522 | en_US |
dc.identifier.issn |
1042-6914 | en_US |
dc.identifier.journal |
MATERIALS AND MANUFACTURING PROCESSES | en_US |
dc.identifier.uri |
http://dx.doi.org/10.1081/AMP-100108522 | en_US |
dc.identifier.uri |
https://ir.lib.nycu.edu.tw/handle/11536/29971 | |
dc.identifier.wosnumber |
WOS:000172665100004 | |
dc.language.iso |
en_US | en_US |
dc.subject |
copper-based composite | en_US |
dc.subject |
density | en_US |
dc.subject |
electrical discharge machining | en_US |
dc.subject |
electrical resistivity | en_US |
dc.subject |
electrode wear ratio | en_US |
dc.subject |
electroless copper plating | en_US |
dc.subject |
fracture surface | en_US |
dc.subject |
hardness | en_US |
dc.subject |
material removal rate | en_US |
dc.subject |
metal matrix composite | en_US |
dc.subject |
porosity | en_US |
dc.subject |
powder metallurgy | en_US |
dc.subject |
silicon carbide | en_US |
dc.subject |
tensile strength | en_US |
dc.subject |
thermal expansion coefficient | en_US |
dc.title |
Fabrication and characterization of Cu-SiCp composites for electrical discharge machining applications | en_US |
dc.type |
Article | en_US |
檔案
- 000172665100004.pdf (898.2 KB, Adobe PDF)
所屬典藏: 期刊論文
引用此條目
Shu, K., & Tu, G. (2001). Fabrication and characterization of Cu-SiCp composites for electrical discharge machining applications. MATERIALS AND MANUFACTURING PROCESSES, 16(4), 483–502. https://doi.org/10.1081/AMP-100108522
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/29971