dc.description.abstractThe instant disclosure relates to a preparation method of ethanol reforming catalyst, comprising the following steps. The first step is mixing a first metal precursor, a second metal precursor, and a third metal precursor with an organic medium to form a mixture. The next step is adding a surfactant to the mixture, and then allowing resting for 3 to 7 days to form a colloidal gel. The next step is calcining the colloidal gel for 1 to 5 hours in a first temperature region of 350° C. to 550° C., and then calcining the colloidal gel for 1 to 5 hours in a second temperature region of 800° C. to 1000° C. to form an ethanol reforming catalyst. The instant disclosure further provides an ethanol reforming catalyst composition.zh_TW
dc.language.isozh_TWen_US
dc.titleETHANOL REFORMING CATALYST COMPOSITION AND METHOD OF PRODUCING ETHANOL REFORMING CATALYSTzh_TW
dc.typePatentsen_US
dc.citation.patentcountryUSAzh_TW
dc.citation.patentnumber20140213440zh_TW
Appears in Collections:Patents


Files in This Item:

  1. 20140213440.pdf

If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.