dc.identifier.urihttp://hdl.handle.net/11536/10875-
dc.description.abstractThe superconducting transition temperatures T-C of face-centered cubic Al1-x-Li-x alloys (x = 0-0.10) exhibit a minimum near x = 0.03 (3 at.% Li). The McMillan strong-coupling T, equation yields a similar trend of the electron-phonon coupling constant.. Meanwhile, the density of states at the Fermi level N(0) decreases monotonically with increasing x. It appears that T-C drops initially due to a reduced N(0), which is then overtaken by alloying-enhanced factors of phonon or electron-phonon interaction. (c) 2007 Elsevier Ltd. All rights reserved.en_US
dc.language.isoen_USen_US
dc.subjectsuperconductorsen_US
dc.subjectelectron-phonon interactionsen_US
dc.titleSuperconducting transition parameters in aluminum-lithium alloys (0-10 at.% Li)en_US
dc.typeArticleen_US
dc.identifier.doi10.1016/j.ssc.2007.03.039en_US
dc.identifier.journalSOLID STATE COMMUNICATIONSen_US
dc.citation.volume142en_US
dc.citation.issue8en_US
dc.citation.spage421en_US
dc.citation.epage424en_US
dc.contributor.department電子物理學系zh_TW
dc.contributor.departmentDepartment of Electrophysicsen_US
dc.identifier.wosnumberWOS:000246997500001-
dc.citation.woscount1-
顯示於類別:期刊論文


文件中的檔案:

  1. 000246997500001.pdf

若為 zip 檔案,請下載檔案解壓縮後,用瀏覽器開啟資料夾中的 index.html 瀏覽全文。