標題: Control ability of spin coating planarization of resist film and optimal control of developers
作者: Kuo, Yang-Kuao
Chao, Chuen-Guang
材料科學與工程學系
Department of Materials Science and Engineering
關鍵字: photolithography;spin coating
公開日期: 1-Aug-2006
摘要: The issue of how to transfer a pattern onto a wafer during photolithography is very important. Normally, the resist is treated as a pattern-transferring medium. Such a medium should have a very smooth surface to reduce the focus error. In this experiment, spin coating is used. The velocity of the center differs from that of the outer edges of a rotating disk, so a perfectly smooth surface cannot be obtained. Therefore, resist temperature, cooling temperature, heating temperature, cup temperature, cup humidity and exhaust pressure were controlled to eliminate this imperfection to yield an acceptable error. A lower cooling temperature yields a thicker center, such that the surface of the wafer protrudes at the center. A lower cooling temperature also corresponds to a thicker center, with the same effect. The cup temperature was set to the cooling temperature so that thickness distribution would be the same as. A higher heating temperature yields a thinner wafer. Higher humidity yields a thinner wafer. (c) 2005 Elsevier Ltd. All rights reserved.
URI: http://dx.doi.org/10.1016/j.mejo.2005.10.009
http://hdl.handle.net/11536/11959
ISSN: 0026-2692
DOI: 10.1016/j.mejo.2005.10.009
期刊: MICROELECTRONICS JOURNAL
Volume: 37
Issue: 8
起始頁: 759
結束頁: 764