dc.description.abstractA two-stage chemical bath deposition (CBD) was reported to modify the thin film deposition of zinc sulfide (ZnS) material, which is a promising candidate as a buffer layer in chalcopyrite solar cells. During the proposed process, two bath temperatures were used subsequently: substrates were immersed in the bath with temperature 85 degrees C for first-stage deposition, followed by the bath with temperature 70 degrees C for the second-stage deposition. As a result, the ZnS film deposited by the proposed two-stage CBD process demonstrated the more desirable film coverage and stoichiometric Zn/S ratio on the soda lime glass substrate than the one without.en_US
dc.language.isoen_USen_US
dc.subjectchemical bath depositionen_US
dc.subjectzinc sulfideen_US
dc.subjectXPS spectrumen_US
dc.subjecttwo-satgeen_US
dc.titleTwo-Stage Chemical Bath Deposition for Well-Covered and Stoichiometric ZnS Thin Filmsen_US
dc.typeProceedings Paperen_US
dc.identifier.journal2012 38TH IEEE PHOTOVOLTAIC SPECIALISTS CONFERENCE (PVSC)en_US
dc.citation.spage1992en_US
dc.citation.epage1994en_US
dc.contributor.department光電工程學系zh_TW
dc.contributor.departmentDepartment of Photonicsen_US
dc.identifier.wosnumberWOS:000309917802062-
Appears in Collections:Conferences Paper