Abstract: Sulfonated dimethyl fumarate (SDMF) was prepared. Poly(ethylene oxide) (PEO) with sodium sulfonate side chains (SPEO) was synthesized by transesterification between SDMF and PEO with molecular weights of 200, 400, 600, 800, and 1000. The SPEO was subsequently mixed as a plasticizer with PEO polyurethane (PU). Samples were characterized by elemental analysis, FTIR, H-1-NMR, gel permeation chromatography, and impedance analysis. The mixture exhibited a homogeneous domain. The maximum conductivity of the CPU1000/SPEO600 was 2.6 x 10(-7) S cm(-1) at room temperature. The relation between the ionic conductivity and the temperature was in agreement with the Arrhenius equation. (C) 2001 John Wiley & Sons, Inc.
URI: http://dx.doi.org/10.1002/app.1880
http://hdl.handle.net/11536/29337
ISSN: 0021-8995
DOI: 10.1002/app.1880
Journal: JOURNAL OF APPLIED POLYMER SCIENCE
Volume: 82
Issue: 3
Begin Page: 541
End Page: 545
Appears in Collections:Articles


Files in This Item:

  1. 000170508700002.pdf

If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.