dc.description.abstractCo-cured materials based on 100/0, 50/50 and 0/100 weight ratios of resole/epoxy were prepared by using NaOH and 4,4'-diaminodiphenylmethane (MDA) as curing agents. Samples were spin-coated on Al plates and were subjected to accelerated aging at 150 degrees C in air for 49 days. The functional group changes during thermal oxidation were monitored with FT-IR at various times. Difference spectra were obtained by using aromatic absorption at 1608 cm(-1) as internal standard. Kinetic study was performed, and a first order of degradation was demonstrated. Experimental results revealed that the degradation rate constants for pure epoxy, 50/50 of resole/epoxy and pure resole are 9.32x10(-3), 4.29x10(-3) and 2.03x10(-3) h(-1), respectively, indicating a significant protection of epoxy against thermal oxidation via co-curing resole/epoxy. (C) 2000 Elsevier Science Ltd. All rights reserved.en_US
dc.language.isoen_USen_US
dc.subjectthermo-oxidationen_US
dc.subjectco-curingen_US
dc.subjectdegradation rate constantsen_US
dc.titleProtection of epoxy resin against thermo-oxidation via co-curing epoxy/resole (I)en_US
dc.typeArticleen_US
dc.identifier.doi10.1016/S0141-3910(00)00058-6en_US
dc.identifier.journalPOLYMER DEGRADATION AND STABILITYen_US
dc.citation.volume69en_US
dc.citation.issue2en_US
dc.citation.spage251en_US
dc.citation.epage253en_US
dc.contributor.department應用化學系zh_TW
dc.contributor.departmentDepartment of Applied Chemistryen_US
dc.identifier.wosnumberWOS:000088241200015-
dc.citation.woscount2-
顯示於類別:期刊論文


文件中的檔案:

  1. 000088241200015.pdf

若為 zip 檔案,請下載檔案解壓縮後,用瀏覽器開啟資料夾中的 index.html 瀏覽全文。