dc.description.abstract | The dependence of morphology of the poly(imide siloxane)s (PISs) on the solubility parameter of unmodified polyimides and the molecular weight and content of alpha,omega-bis(3-aminopropyl) polydimethylsiloxane (APPS) has been studied. The effect of the morphology on the mechanical properties is also under investigation. The domain formation in the PISs with the APPS molecular weight M-n = 507 g/mol is not found until the mol ratio of APPS/PIS greater than or equal to 0.5% in the pyromellitic dianhydride/p-phenylene diamine (PMDA/p-PDA)-based PISs, and at a mol ratio greater than or equal to 2.7% in the 3,3',4,4'-benzophenone tetracarboxylic dianhydride/2,2'-bis[4-(3-aminophenoxy)phenyl] sulfone (BTDA/m-BAPS)-based PISs. As the APPS M-n = 715 g/mol, the critical APPS concentrations of the domain formation in both types of PISs are equal to 0.1 and 1.1%, respectively. The critical concentration is equal to 0.6% in the BTDA/m-BAPS-based PIS film with the APPS M-n = 996 g/mol. The isolated siloxane-rich phase in the BTDA/m-BAPS-based PISs becomes a continuous phase as the ,ol ratio of APPS/PIS greater than or equal to 7.7, 10.0, and 16.6% as the APPS M-n = 996, 715, and 507 g/mol, respectively. Dynamic Mechanical Analysis (DMA) shows two T(g)s in the PIS films having phase separation: one at -118 similar to -115 degrees C, being the siloxane-rich phase, the other at 181-244 degrees C, being the aromatic imide-rich phase. The SEM micrographs show a significant deformation on the fractured surfaces of the BTDA/m-BAPS-based PIS films with a continuous siloxane-rich phase. This phenomenon of plastic deformation is also observed in the tensile tests at -118 degrees C and at room temperature. The highest elongation in the PIS films is found at the critical siloxane content of the continuous siloxane-rich phase formation. (C) 1999 John Wiley & Sons, Inc. J Appl Polym Sci 74: 2832-2847, 1999. | en_US |
dc.language.iso | en_US | en_US |
dc.subject | poly(imide siloxane)s | en_US |
dc.subject | morphology | en_US |
dc.subject | phase separation | en_US |
dc.subject | plastic deformation | en_US |
dc.title | Effects of the solubility parameter of polyimides and the segment length of siloxane block on the morphology and properties of poly(imide siloxane) | en_US |
dc.type | Article | en_US |
dc.identifier.doi | 10.1002/(SICI)1097-4628(19991213)74:12<2832 | en_US |
dc.identifier.journal | JOURNAL OF APPLIED POLYMER SCIENCE | en_US |
dc.citation.volume | 74 | en_US |
dc.citation.issue | 12 | en_US |
dc.citation.spage | 2832 | en_US |
dc.citation.epage | 2847 | en_US |
dc.contributor.department | 材料科學與工程學系 | zh_TW |
dc.contributor.department | Department of Materials Science and Engineering | en_US |
dc.identifier.wosnumber | WOS:000083310300007 | - |
dc.citation.woscount | 18 | - |
顯示於類別: | 期刊論文 |