dc.contributor.author張曜洲en_US
dc.contributor.authorYao-Chou Changen_US
dc.contributor.author許海龍en_US
dc.contributor.authorDr. Hai-Lung Hsuen_US
dc.date.accessioned2014-12-12T02:10:10Z-
dc.date.available2014-12-12T02:10:10Z-
dc.date.issued1992en_US
dc.identifier.urihttp://140.113.39.130/cdrfb3/record/nctu/#NT810015042en_US
dc.identifier.urihttp://hdl.handle.net/11536/56559-
dc.description.abstract試驗結果顯示,不論疏鬆狀態或中等緊密狀態及緊密狀態,發現當爐石含量 佔60%時為抗液化強度之轉折點,此現象供為工程規劃設計之依據.zh_TW
dc.language.isozh_TWen_US
dc.subject爐石zh_TW
dc.subjectBlast Furnace Slagen_US
dc.title爐石與砂土混合料之動態行為研究zh_TW
dc.titlePrimary Study Of Dynamic Behavior For Composite Of Blast Furnace lag And Sanden_US
dc.typeThesisen_US
dc.contributor.department土木工程學系zh_TW