DC 欄位 | 值 | 語言 |
---|---|---|
dc.contributor.author | 張曜洲 | en_US |
dc.contributor.author | Yao-Chou Chang | en_US |
dc.contributor.author | 許海龍 | en_US |
dc.contributor.author | Dr. Hai-Lung Hsu | en_US |
dc.date.accessioned | 2014-12-12T02:10:10Z | - |
dc.date.available | 2014-12-12T02:10:10Z | - |
dc.date.issued | 1992 | en_US |
dc.identifier.uri | http://140.113.39.130/cdrfb3/record/nctu/#NT810015042 | en_US |
dc.identifier.uri | http://hdl.handle.net/11536/56559 | - |
dc.description.abstract | 試驗結果顯示,不論疏鬆狀態或中等緊密狀態及緊密狀態,發現當爐石含量 佔60%時為抗液化強度之轉折點,此現象供為工程規劃設計之依據. | zh_TW |
dc.language.iso | zh_TW | en_US |
dc.subject | 爐石 | zh_TW |
dc.subject | Blast Furnace Slag | en_US |
dc.title | 爐石與砂土混合料之動態行為研究 | zh_TW |
dc.title | Primary Study Of Dynamic Behavior For Composite Of Blast Furnace lag And Sand | en_US |
dc.type | Thesis | en_US |
dc.contributor.department | 土木工程學系 | zh_TW |