標題: | Investigation of the interactions between titanium and calcium zirconium oxide (CaZrO3) ceramics modified with alumina |
作者: | Lu, Ming-Wei Lin, Kun-Lin Lin, Chien-Cheng 材料科學與工程學系 Department of Materials Science and Engineering |
關鍵字: | titanium casting;CaZrO3;Ca3Al2O6;microstructure;phase identification |
公開日期: | 1-Jan-2019 |
摘要: | Powdered mixtures of CaO, ZrO2 and Al2O3 in various ratios were hot pressed. The mixtures reacted with titanium at 1600 degrees C for 30 min in argon to evaluate the suitable ceramic crucibles for casting of titanium. The interfacial microstructures between titanium and ceramic composites were characterized using X-ray diffractometer, scanning and transmission electron microscope. The produced hot pressed mixtures that were chemically bonded together, contained calcium aluminate (CaAl2O4), calcium dialuminate (CaAl4O7), cubic zirconia (c-ZrO2), and calcium zirconium oxide (CaZrO3). The increase in Al2O3 amount led to the decrease in CaZrO3 amount and an increase in the amount of CaAl2O4, CaAl4O7 and c-ZrO2 due to the reaction of CaO and Al2O3. At the end of the reaction of the ceramic mixtures with Ti at 1600 degrees C for 30 min, the acicular alpha-Ti and beta'-Ti were formed at the interface of Ti and the composites containing up to 10 vol.% Al O-2(3). In composites containing more than 20 vol.% Al2O3, Ti3Al5 was found at the interface instead of alpha-Ti and beta'-Ti. Furthermore, CaZrO3, ZrO2 and Ca3Al2O6 existed on the sides of the ceramic far away from the interface. CaZrO3/Al2O3 composites with less than 20 vol.% Al2O3 could be a potential crucible or mould material for productive applications in titanium casting. |
URI: | http://dx.doi.org/10.2298/PAC1901079L http://hdl.handle.net/11536/151653 |
ISSN: | 1820-6131 |
DOI: | 10.2298/PAC1901079L |
期刊: | PROCESSING AND APPLICATION OF CERAMICS |
Volume: | 13 |
Issue: | 1 |
起始頁: | 79 |
結束頁: | 88 |
Appears in Collections: | Articles |