標題: | Defects in semipolar (11(2)over-bar(2)over-bar) ZnO grown on (112) LaAlO3/(La, Sr) (Al, Ta)O-3 substrate by pulsed laser deposition |
作者: | Tian, Jr-Sheng Wu, Yue-Han Peng, Chun-Yen Chiu, Kun-An Shih, Yi-Sen Do, Hien Lin, Pei-Yin Ho, Yen-Teng Chu, Ying-Hao Chang, Li 材料科學與工程學系 Department of Materials Science and Engineering |
公開日期: | 27-Mar-2013 |
摘要: | The microstructure of semipolar (11 (2) over bar(2) over bar) ZnO deposited on (112) LaAlO3/(La, Sr) (Al, Ta)O-3 was investigated by transmission electron microscopy. The ZnO shows an in-plane epitaxial relationship of [11 (2) over bar3](ZnO) parallel to [11 (1) over bar](LAO/LSAT) with oxygen-face sense polarity. The misfit strain along [11 (2) over bar3](ZnO) and [1 (1) over bar 00](ZnO) is relieved through the formation of misfit dislocations with the Burgers vectors b = 1/6[11 (2) over bar3](ZnO) and b = 1/3 < 1 (2) over bar 10 >(ZnO), respectively. The line defects in the semipolar ZnO are predominantly perfect dislocations, and the dislocation density decreases with increasing ZnO thickness as a result of dislocation reactions. Planar defects were observed to lie in the M-plane and extend along < 0001 >, whereas basal stacking faults were rarely found. |
URI: | http://dx.doi.org/10.1088/0953-8984/25/12/125801 http://hdl.handle.net/11536/21372 |
ISSN: | 0953-8984 |
DOI: | 10.1088/0953-8984/25/12/125801 |
期刊: | JOURNAL OF PHYSICS-CONDENSED MATTER |
Volume: | 25 |
Issue: | 12 |
結束頁: | |
Appears in Collections: | Articles |
Files in This Item:
If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.