標題: The characteristics and engineering properties of dry-mix/steam-injection concrete
作者: Su, N
Peng, YN
土木工程學系
Department of Civil Engineering
關鍵字: concrete;steam;dry mixture;compressive strength
公開日期: 1-Apr-2001
摘要: This study aims to investigate the characteristics and engineering properties of the dry-mix/steam-injection method (DMSIM) which was developed to overcome difficulties involved in vacuum conditions of the lunar environment. A comparison was made to examine the differences in the hydration process, mechanical properties and the composition of hydration products between DMSIM and the normal-temperature wet-mix method (NTWMM). In DMSIM. when dry cement particles come in contact with steam, heal immediately transfers from the steam to the cement, with part of the steam being forced into the inner regions of the cement particles via the micropores. As cement particles gain activation energy and moisture condensed from steam? they undergo rapid and complete hydration. Test results showed that the optimal steaming temperature for dry-mix samples of cement and standard sand is 180-200 degreesC and the optimal steaming scenario for 10 cm(3) samples of concrete is at 200 degreesC for 18 h. The present DMSIM has advantages of lower cement content, shorter hardening time and higher concrete strengths, as compared to NTWMM. (C) 2001 Elsevier Science Ltd. Ail rights reserved.
URI: http://dx.doi.org/10.1016/S0008-8846(01)00460-4
http://hdl.handle.net/11536/29725
ISSN: 0008-8846
DOI: 10.1016/S0008-8846(01)00460-4
期刊: CEMENT AND CONCRETE RESEARCH
Volume: 31
Issue: 4
起始頁: 609
結束頁: 619