標題: Wafer bonding by low-temperature soldering
作者: Lee, C
Huang, WF
Shie, JS
光電工程學系
Department of Photonics
關鍵字: wafer bonding;soldering;sealing;package;microsensors
公開日期: 25-Aug-2000
摘要: Recently. wafer level packaging received lots of attention in microsystems because it shows the potential to reduce the packaging cost, while the yield of devices after dicing and packaging can be increased. However, there is a limitation of commercialized wafer bonding technology. i.e., the high process temperature, such as 1000 degrees C of silicon fusion bonding, and 450 degrees C of anodic bonding. A novel tow-temperature wafer bonding with process temperature lower than 160 degrees C is proposed, it applies the In-Sn alloy to form the interface of wafer bonding. The experiment results show helium leak test of 6 x 10(-9) Torr 1/s, and a tensile strength as high as 200 kg/cm(2). Reliability test after 1500 temperature cycles between -10 degrees C and 80 degrees C also shows no trace of degradation compared to the initial quality of the samples. This low-temperature soldering process demonstrates its promising potential at the wafer level packaging in industrial production. (C) 2000 Elsevier Science. S.A. All rights reserved.
URI: http://dx.doi.org/10.1016/S0924-4247(00)00338-1
http://hdl.handle.net/11536/30325
ISSN: 0924-4247
DOI: 10.1016/S0924-4247(00)00338-1
期刊: SENSORS AND ACTUATORS A-PHYSICAL
Volume: 85
Issue: 1-3
起始頁: 330
結束頁: 334
Appears in Collections:Conferences Paper


Files in This Item:

  1. 000089375900053.pdf