標題: | Effects of the solubility parameter of polyimides and the segment length of siloxane block on the morphology and properties of poly(imide siloxane) |
作者: | Jwo, SL Whang, WT Liaw, WC 材料科學與工程學系 Department of Materials Science and Engineering |
關鍵字: | poly(imide siloxane)s;morphology;phase separation;plastic deformation |
公開日期: | 13-Dec-1999 |
摘要: | The dependence of morphology of the poly(imide siloxane)s (PISs) on the solubility parameter of unmodified polyimides and the molecular weight and content of alpha,omega-bis(3-aminopropyl) polydimethylsiloxane (APPS) has been studied. The effect of the morphology on the mechanical properties is also under investigation. The domain formation in the PISs with the APPS molecular weight M-n = 507 g/mol is not found until the mol ratio of APPS/PIS greater than or equal to 0.5% in the pyromellitic dianhydride/p-phenylene diamine (PMDA/p-PDA)-based PISs, and at a mol ratio greater than or equal to 2.7% in the 3,3',4,4'-benzophenone tetracarboxylic dianhydride/2,2'-bis[4-(3-aminophenoxy)phenyl] sulfone (BTDA/m-BAPS)-based PISs. As the APPS M-n = 715 g/mol, the critical APPS concentrations of the domain formation in both types of PISs are equal to 0.1 and 1.1%, respectively. The critical concentration is equal to 0.6% in the BTDA/m-BAPS-based PIS film with the APPS M-n = 996 g/mol. The isolated siloxane-rich phase in the BTDA/m-BAPS-based PISs becomes a continuous phase as the ,ol ratio of APPS/PIS greater than or equal to 7.7, 10.0, and 16.6% as the APPS M-n = 996, 715, and 507 g/mol, respectively. Dynamic Mechanical Analysis (DMA) shows two T(g)s in the PIS films having phase separation: one at -118 similar to -115 degrees C, being the siloxane-rich phase, the other at 181-244 degrees C, being the aromatic imide-rich phase. The SEM micrographs show a significant deformation on the fractured surfaces of the BTDA/m-BAPS-based PIS films with a continuous siloxane-rich phase. This phenomenon of plastic deformation is also observed in the tensile tests at -118 degrees C and at room temperature. The highest elongation in the PIS films is found at the critical siloxane content of the continuous siloxane-rich phase formation. (C) 1999 John Wiley & Sons, Inc. J Appl Polym Sci 74: 2832-2847, 1999. |
URI: | http://hdl.handle.net/11536/30903 http://dx.doi.org/10.1002/(SICI)1097-4628(19991213)74:12<2832 |
ISSN: | 0021-8995 |
DOI: | 10.1002/(SICI)1097-4628(19991213)74:12<2832 |
期刊: | JOURNAL OF APPLIED POLYMER SCIENCE |
Volume: | 74 |
Issue: | 12 |
起始頁: | 2832 |
結束頁: | 2847 |