dc.description.abstractThis work studied the morphology and annealing behaviors of extended defects in Si subjected to various Ge+ preamorphization and BF2+ implantation conditions. The extended defects formed were near the specimen surface when Ge+ implantation energy and dose amount were low. During subsequent annealing, the end-of-range (EOR) loops were enlarged and then moved out of the specimen. High energy/low dose Ge+ implantation generated a damaged layer which initially transformed into a wide zone containing dislocation loops and rodlike defects in the annealed specimen. As the annealing proceeded, the width of defective zone gradually shrunk so that most of the extended defects could be annihilated by defect rejection/recombination process. In addition to the category II defects found in previous investigations, hairpin dislocations emerged in high energy/high dose Ge+-implanted specimens. In this specimen, rodlike defects and hairpin dislocations could be removed by annealing, while the EOR loops became relatively inert so that their removal would require high temperatures and/or long annealing times. Microwave plasma surface treatment was also carried out to form a nitride layer on specimen surface. Experimental results indicate that in addition to effectively reducing the size of EOR loops, surface nitridation might serve as a vacancy source injecting vacancies into Si to annihilate the interstitials bounded by dislocation loops. Reduction in the defect size was pronounced when bias voltage was added to the plasma process. However, radiation damage might occur with too high of a bias voltage. (C) 1999 American Institute of Physics. [S0021-8979(99)06322-7].en_US
dc.language.isoen_USen_US
dc.titleDefects in Ge+-preamorphized siliconen_US
dc.typeArticleen_US
dc.identifier.journalJOURNAL OF APPLIED PHYSICSen_US
dc.citation.volume86en_US
dc.citation.issue10en_US
dc.citation.spage5399en_US
dc.citation.epage5406en_US
dc.contributor.department材料科學與工程學系zh_TW
dc.contributor.departmentDepartment of Materials Science and Engineeringen_US
dc.identifier.wosnumberWOS:000083435900011-
dc.citation.woscount0-
顯示於類別:期刊論文


文件中的檔案:

  1. 000083435900011.pdf

若為 zip 檔案,請下載檔案解壓縮後,用瀏覽器開啟資料夾中的 index.html 瀏覽全文。