標題: | Compatibilization and elastomer toughening of polyamide-6 (PA6)/poly(phenylene ether) (PPE) blends |
作者: | Chiou, KC Wu, SC Wu, HD Chang, FC 應用化學系 Department of Applied Chemistry |
關鍵字: | PA6;PPE;SMA;toughness;compatibilizer;impact modifier |
公開日期: | 3-Oct-1999 |
摘要: | In the elastomer-modified (polyamide-6/poly(phenylene ether) (PA6/PPE) = 50/50 blends, poly(styrene-co-maleic anhydride) (SMA) was demonstrated to be an efficient reactive compatibilizer. The G1651 elastomer was shown to be an effective impact modifier to result in superior toughness and heat-deflection temperature (HDT) than is the 1901X elastomer for the SMA-compatibilized blends because G1651 particles exclusively reside within the dispersed PPE phase but 1901X particles tend to distribute in the PA6 matrix and/or along the interface. The apparent average diameter of the dispersed PPE phase is insignificantly dependent on the elastomer content in the G1651-modified blend, whereas it increases with increase of the elastomer content in the 1901X-modified blend. Moreover, there exists a critical elastomer content, 15 phr, for the ductile-brittle transition of the G1651-modified SMA-modified PA6/PPE blends. (C) 1999 John Wiley & Sons, Inc. |
URI: | http://hdl.handle.net/11536/31037 |
ISSN: | 0021-8995 |
期刊: | JOURNAL OF APPLIED POLYMER SCIENCE |
Volume: | 74 |
Issue: | 1 |
起始頁: | 23 |
結束頁: | 32 |
Appears in Collections: | Articles |
Files in This Item:
If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.