標題: Effect of temperature on fracture toughness of PC/ABS based on J-integral and hysteresis energy methods
作者: Lu, ML
Chiou, KC
Chang, FC
應用化學系
Department of Applied Chemistry
公開日期: 7-十一月-1996
摘要: The critical fracture toughness J(1c) of the polycarbonate (PC)/acrylonitrile-butadiene-styrene (ABS) blend at different temperatures was obtained from ASTM E813-81, E813-87, and the recently developed hysteresis energy methods, respectively. The J(1c) value increases with increase of the test temperature ranging from -60 to 70 degrees C. The hysteresis energy method and the ASTM E813-81 method result in comparable J(1c) values, while the ASTM E813-87 results in about 80-110% higher values. The critical initiation displacements determined from the plots of hysteresis energy and the true crack growth length vs. crosshead displacement are very close. This indicates that the critical initiation displacement deter mined by the hysteresis method is indeed the displacement at the onset of true crack initiation and the corresponding J(1c) represents a physical event of crack initiation. The fracture toughness, K-1c value, based on linear elastic fracture mechanics (LEFM), was determined by using K-Q analysis (ASTM E399-78), and the obtained K-Q value decreases with the increase of the test temperature. The K-Q value is not the real LEFM K-1c value because the criterion of P-max/P-Q < 1.1 has not been satisfied. However, the corresponding J(Q) obtained from the K-Q analysis is comparable to the J(1c) obtained from the E813-81 method at lower temperature (-45 or -60 degrees C), an indication of LEFM behavior at lower temperature. The various schemes and size criterion based on LEFM and the J-method are explored for the validity of J(1c) and K-1c values. (C) 1996 John Wiley & Sons, Inc.
URI: http://hdl.handle.net/11536/931
ISSN: 0021-8995
期刊: JOURNAL OF APPLIED POLYMER SCIENCE
Volume: 62
Issue: 6
起始頁: 863
結束頁: 874
顯示於類別:期刊論文


文件中的檔案:

  1. A1996VL69200002.pdf

若為 zip 檔案,請下載檔案解壓縮後,用瀏覽器開啟資料夾中的 index.html 瀏覽全文。