Temperature dependent integrity of Sr0.8Bi2Ta2O9 films on ultra-thin Al2O3 buffered Si

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

DOI

10.1016/S0254-0584(02)00517-5

Abstract

The annealing temperature dependent integrity of Sr0.8Bi2Ta2O9 (SBT) on ultra-thin 4 nm SiO2 and Al2O3 buffered Si was investigated in this work. Although the capacitance-voltage characteristics show hysteresis loops in both cases, the memory window of Sr0.8Bi2Ta2O9/Al2O3 capacitor is larger than that of Sr0.8Bi2Ta2O9/SiO2 capacitor. As increasing annealing temperature from 800 to 900degreesC, the grain size and memory window of polycrystalline SBT increase both cases. At 800degreesC, the leakage current density of Sr0.8Bi2Ta2O9/Al2O3 capacitor is 3.2 x 10(-8) A/cm(2) at -3V, which is low enough for deep sub-mum application. With increasing temperature to 900degreesC, the leakage current in both structures becomes smaller. (C) 2002 Elsevier Science B.V. All rights reserved.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By