Formation of NiSi-silicided p(+)n shallow junctions by BF2+ implantation into/through silicide and rapid thermal annealing

檔案

本條目沒有附加檔案。

至出版者網站查看(DOI) ›

日期

2005-01-01

類型

期刊名稱

JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS

卷期與頁次

第 44 卷,頁 108–113

ISSN

0021-4922

語言

英文

摘要

NiSi-silicided p(+) n shallow junctions are fabricated by BF2+ implantation into/through a thin NiSi silicide layer, followed by rapid thermal annealing (RTA). The NiSi film starts to show agglomeration after RTA at 650degreesC, which may result in the formation of discontinuous islands at higher temperatures. The incorporation of fluorine atoms in the NiSi film can retard the film agglomeration making the film stable up to 800degreesC. A forward ideality factor very close to unity and a reverse bias current density of 0.6 nA/cm(2) can be attained for the NiSi(31 nm)/p(+)n junctions fabricated by BF2+ implantation to a dose of 5 x 10(15) cm(-2) at 35 keV, followed by RTA for 30 s at 650degreesC; the junction formed is about 37 nm measured from the NiSi/Si interface. Activation energy measurement shows that the reverse bias junction currents are dominated by the diffusion current, which indicates that most of the implanted damage can be recovered by RTA at temperatures as low as 650degreesC.

所屬典藏

期刊論文
顯示完整詮釋資料 統計資料

引用此條目

Wang, C., Wu, Y., Wu, W., & Chen, M. (2005). Formation of NiSi-silicided p(+)n shallow junctions by BF2+ implantation into/through silicide and rapid thermal annealing. JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 44, 108–113. https://doi.org/10.1143/JJAP.44.108

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://ir.lib.nycu.edu.tw/handle/11536/148869