Variation of electrical properties of Sro(0.8)Bi(2+x)Ta(2)O(9+delta) ferroelectric thin films with bismuth content
檔案
本條目沒有附加檔案。
日期
2003
期刊名稱
ADVANCED CERAMICS AND COMPOSITES
卷期與頁次
第 247 卷,頁 381–384
ISSN
1013-9826
ISBN
0-87849-924-5
語言
英文
摘要
In this work, we have investigated the effect of bismuth content on electrical properties of Sr0.8Bi2+xTa2O9+delta (SBT) thin films, obtained by using the metallorganic decomposition technique. The SBT precursor solution was prepared using high purity strontium acetate, bismuth acetate and tantalum ethoxide as the starting materials and acetic acid as the solvent. Thin films were deposited on Ir(50nm)/SiO2(100Mn)/Si substrates by spin coating with precise control of the solution viscosity and spin speed. As-deposited films were dried at 150degreesC for 10 min followed by pyrolysis at 400degreesC for 30 min in static air to remove the solvent and organic impurities. The films were then post-annealed at 650degreesC for 30 min in ambient oxygen atmosphere. The crystallinity of SBT thin films containing various bismuth levels was characterized by X-ray diffraction (XRD). The 30% Bi excess SBT thin films exhibited preferentially (115) oriented phase. The XRD pattern showed all major peaks corresponding to SBT phase. The microstructure, P-E hysteresis loops and leakage current of SBT films were found to be dependent on the bismuth content.
所屬典藏
會議論文引用此條目
Chou, H., Tseng, T., & Chen, T. (2003). Variation of electrical properties of Sro(0.8)Bi(2+x)Ta(2)O(9+delta) ferroelectric thin films with bismuth content. ADVANCED CERAMICS AND COMPOSITES, 247, 381–384. https://ir.lib.nycu.edu.tw/handle/11536/28288
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://ir.lib.nycu.edu.tw/handle/11536/28288