標題: | 氮化鈦與鈦金屬界面反應之微觀結構分析 Microstructural Characterization of Interface Reaction between Titanium Nitride and Titanium |
作者: | 蘇桓德 林健正 材料科學與工程學系 |
關鍵字: | 氮化鈦;界面反應;微觀結構;鈦金屬;Titanium nitride;Interface Reaction;Microstructural Characterization;Titanium |
公開日期: | 2004 |
摘要: | 氮化鈦(Titanium nitride, TiN)/鈦(Titanium, Ti)在1atm Ar氣氛下進行1000~1500℃各種不同時間之擴散反應,利用X光繞射(x-ray diffraction, XRD)、掃描式電子顯微鏡(scanning electron microscopy/energy dispersive spectroscopy, SEM/EDS)與穿透式電子顯微鏡(TEM/EDS),分析擴散反應後界面之顯微結構。TiN/Ti在1000℃/36hrs界面反應後,反應生成物從TiN側至Ti側為ε-TiN(tetragonal),經1300℃/36hrs擴散反應後,反應生成物從TiN側至Ti側依序為ε-TiN(tetragonal)與α-TiN0.3(hexagonal),其中ε-TiN是經由包析反應所產生,在1400℃/36hrs擴散反應時,又析出針狀Ti2N,經過1500℃/36hrs擴散反應後,α-TiN0.3並沒出現,但卻在兩相區中出現長板狀的析出物α-Ti。 In this work, the interfacial reactions in the TiN/Ti diffusion couple were investigated. TiN/Ti diffusion couples were annealed at temperatures ranging from 1000 to 1500℃in argon atmosphere for 36hours. The microstructures of the reaction interface were characterized using x-ray diffraction (XRD), scanning electron microscopy (SEM), and analytical transmission electron microscopy (TEM/EDS). Phases of ε-TiN(tetragonal) was observed from TiN-side to Ti-side of the diffusion couple after reaction at 1000℃ for 36 hours. After reaction at 1300℃ for 36 hours , ε-TiN(tetragonal) and α-TiN0.3(hexagonal)were observed from TiN-side to Ti-side, and ε-TiN were formed by the peritectoid reaction. However, after reaction at 1400℃ for 36 hours, the needle-like Ti2N was precipitated. Finally, α-TiN0.3 did not exist after reaction at 1500℃ for 36 hours, but lath-like α-Ti was precipitated in the two-phase region. |
URI: | http://140.113.39.130/cdrfb3/record/nctu/#GT009218506 http://hdl.handle.net/11536/74602 |
顯示於類別: | 畢業論文 |