標題: | Self-constraining method for low shrinkage of low-temperature-cofired ceramic devices |
作者: | Jao, Jui-Chu Lin, Pang 材料科學與工程學系 Department of Materials Science and Engineering |
關鍵字: | LTCC;low shrinkage;self-constraining;CaO-SiO2 glass;onset shrinkage temperature |
公開日期: | 1-Jun-2007 |
摘要: | A new technique developed for the low shrinkage of low-temperature-cofired-ceramics (LTCCs) is proposed; this technique is based on a self-constraining mechanism, which relies on composite green tapes formed by two laminated glass layers, each of which has a distinct softening point (onset shrinkage temperature, OST) and a crystallization temperature (CRT). Each layer works as a constraining layer for the other layer in a distinct temperature range to prevent excessive linear shrinkage along the layer plane. The OSTs ranging from 802 to 606 degrees C are adjusted by controlling the amount of Na2O (0-1.0 wt %) added to the CaO-SiO2 glass. The OST and CRT of the two glass layers as well as the heating profile have strong effects on shrinkage ratio, the lowest of which is found to be only 0.2% after sintering up to 880 degrees C. The measured dielectric constant of the sintered samples is approximately 6.0 within a narrow variation range even when the samples have a wide range of shrinkage ratios. |
URI: | http://dx.doi.org/10.1143/JJAP.46.3654 http://hdl.handle.net/11536/10770 |
ISSN: | 0021-4922 |
DOI: | 10.1143/JJAP.46.3654 |
期刊: | JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS |
Volume: | 46 |
Issue: | 6A |
起始頁: | 3654 |
結束頁: | 3657 |
Appears in Collections: | Articles |
Files in This Item:
If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.