摘要: NiSi-silicided n(+)p shallow junctions are fabricated by P+/F+ dual implantation into/through a thin NiSi silicide layer followed by low-temperature furnace annealing. The incorporation of fluorine atoms in the 61-nm-thick NiSi film retards film agglomeration, making the film stable up to 750 degrees C for 90 min. A forward ideality factor of 1.08 and a reverse bias current density (at 5 V) of 0.7 nA/cm(2) can be attained for the NiSi (61 nm)/n(+)p junctions with an area of 580 x 580 mu m(2) fabricated by P+/F+ dual implantation at 35/30 keV to a close of 5 x 10(15) 15 x 10(15) cm(-2) followed by 750 degrees C thermal annealing. The junction formed is about 71 nm from the NiSi/Si interface. Activation energy measurement shows that the reverse bias area current of the NiSi/n(+)p junctions is dominated by the diffusion current, while their reverse bias peripheral Current is dominated by the minority generation Current at room temperature. This implies the presence of generation centers in and/or close to the junction region along the perimeter.
URI: http://dx.doi.org/10.1143/JJAP.45.1582
http://hdl.handle.net/11536/12593
ISSN: 0021-4922
DOI: 10.1143/JJAP.45.1582
期刊: JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS
Volume: 45
Issue: 3A
起始頁: 1582
結束頁: 1587
顯示於類別:期刊論文


文件中的檔案:

  1. 000236191900021.pdf

若為 zip 檔案,請下載檔案解壓縮後,用瀏覽器開啟資料夾中的 index.html 瀏覽全文。