標題: | Chemical stability of embedded material for attenuated phase-shifting mask and application of high-transmittance attenuated phase-shifting mask for 0.1 mu m contact pattern in 193 nm lithography |
作者: | Lin, CM Loong, WA 應用化學系 Department of Applied Chemistry |
關鍵字: | chemical stability;sputtering condition;attenuated phase-shifting mask;dark tone;side lobe;chemically amplified resist;high transmittance |
公開日期: | 1-Jun-2002 |
摘要: | When the compositions of Al2O3. SiO2., and other oxides were increased, refractive index (n) appeared to increase and extinction coefficient (k) to decrease in AlSixOy. The study of the correlation among sputtering conditions, chemical compositions and optical properties could lead to the chemical stability of AlSixOy embedded material. Bi layer AlSixOy thin film may be a new high-transmittance (T% similar to 35%) embedded layer of attenuated phase-shifting masks (AttPSMs) in 193 nm lithography, The transparent layer with saturation of Al2O3 and SiO2 compositions exhibits n of 2.3-2.4 and k of 0.1-0.2. The absorptive layer with higher concentrations of Al and Si exhibits n of 1.5-1.7 and k of 0.3-0.4. Combining a dark-tone mask, high-transmittance AttPSM and negative resist resulted in better contrast of the aerial image and a resolution of 0.1 mum for the contact-hole pattern in 193 nm lithography, A 0.20-mum-line/space (1: 1) etched pattern was successfully fabricated using AlSixOy, as an embedded layer. |
URI: | http://dx.doi.org/10.1143/JJAP.41.4037 http://hdl.handle.net/11536/28774 |
ISSN: | 0021-4922 |
DOI: | 10.1143/JJAP.41.4037 |
期刊: | JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS |
Volume: | 41 |
Issue: | 6B |
起始頁: | 4037 |
結束頁: | 4041 |