摘要: | Sputter clean had been accepted as an effective surface clean process prior to metal deposition. In this work, the impact of interface nature on via resistance of Al-interconnect as via size is scaled down to 0.16 mum was studied. Al-F compound was identified as the main interfacial contaminants after standard post-etch clean process if the TiN laver of the underlying metal line were etched through during via etch. For via size larger than 0.25 mum (aspect ratio lower than 3.2), Al-F compound can be removed by sputter clean effectively. However, below 0.25 mum, sputter clean efficiency decreases such that via resistance is degraded by the existence of Al-F interfacial layer. On the other hand, sputter clean results in oxide re-deposition, which in turn degrades via resistance. It is suggested that to obtain low resistance sub-0.2 mum via, via etch must stop on TiN layer such that no Al-F layer can be formed. Otherwise, new interfacial layer clean technology with high efficiency and without side effect has to be developed. (C) 2001 Elsevier Science Ltd. All rights reserved. |
URI: | http://dx.doi.org/10.1016/S0026-2714(01)00090-7 http://hdl.handle.net/11536/29316 |
ISSN: | 0026-2714 |
DOI: | 10.1016/S0026-2714(01)00090-7 |
期刊: | MICROELECTRONICS RELIABILITY |
Volume: | 41 |
Issue: | 11 |
起始頁: | 1889 |
結束頁: | 1896 |
Appears in Collections: | Conferences Paper |
Files in This Item:
If it is a zip file, please download the file and unzip it, then open index.html in a browser to view the full text content.